Our Stocks are indicated in the tables below. Standard sizes not in our stocks can be requested
EN-36c STEELS
Ni-cr-mo steel
Approximate Other Equivalents

IS : 13 Ni 113 Cr 3 VISL : MES SPL MO BS : 655 M13

AISI : 3310

APPLICATION

Heavy Duty Gearings, Air Craft & Transport Vehicle construction Button Bits for Borwell Boring, Automobile Transmission Parts.,

Our Colour Code: BLUE

LIST OF STANDARD SIZES

  • Round: Ø 16mm – Ø 300mm

OUR STOCKS

  • Round: Ø 16mm – Ø 200mm
QUALITYCSIMNCRNiMoP & S
EN – 36C0.10.10.30.630.150.055
0.150.350.613.750.25MAX
SPECIFIC HEAT TREATMENT
QUALITYEN – 36 C
Forging Temperature1100 to 850ºC
Annealing Temperature640 to 660ºC (Soft Annealing)
Annealed Hardness BHN Max217 BHN
Hardening Temperature830 to 850ºC, 700 to 800ºC R & H
Quenching MediaOil Salt Bath at 180 to 250ºC
Obtainable Hardness R.C.—-
Working Hardness HRC.—-
Tempering Temperature170 to 200ºC
Mormalising Temperature850 to 880ºC
EN-207 STEELS / 20Mncr5 & 16Mncr5
Cr-Mn Steel
APPROXIMATE OTHER EQUIVALENTS

IS: 16 MnCr4/15 Cr5   VISL: MEB 60 (20Cr5)   80 (16MnCr5)
DIN: 15Cr3, 16MnCr5/20MnCr5 ASI: 5120 ASP: EN 207 (15Cr3)

APPLICATION

15Cr3: Small Parts with medium core strength & good wear Resistance Piston Rings, Bushes, Drilling Machine Spindles.
15 MnCr5 & 20MnCr5: Parts subject to medium stress but with high wear such as gear wheel steering of vehicles & general engineering work

Our Colour Code: WHITE & BLUE

LIST OF STANDARD SIZES

  • 20MnCr5 Round: Ø 16mm – Ø 285mm
  • Square: 6mm to 300mm

OUR STOCKS

  • 20MnCr5 Round: Ø 16mm – Ø 200mm 
  • Square: 65mm to 100mm
QUALITYCSiMnCrP & S
15Cr30.120.150.40.40.55
15Cr30.180.40.60.7MAX
16MnCr50.140.1510.81.55
16MnCr50.190.41.31.1MAX
20MnCr50.160.1510.92.55
20MnCr50.230.41.41.1MAX
SPECIFIC HEAT TREATMENT
QUALITY15 Cr 316 Cr 317 Cr 3
Forging Temperature1100 to 850ºC1101 to 850ºC1102 to 850ºC
Annealing Temperature650 to 700ºC (Soft Annealing)651 to 700ºC (Soft Annealing)652 to 700ºC (Soft Annealing)
Annealed Hardness BHN Max200 BHN207 BHN217 BHN
Hardening Temperature830 to 850ºC831 to 850ºC832 to 850ºC
Quenching MediaOil / Salt Bath | Air180 to 250ºCOil / Salt Bath | Air180 to 250ºCOil / Salt Bath | Air180 to 250ºC
Obtainable Hardness R.C.—-—-—-
Working Hardness HRC.—-—-—-
Tempering Temperature150 to 180ºC170 to 200ºC170 to 200ºC
Normalising Temperature870 to 900ºC870 to 890ºC860 to 890ºC
EN-353 & 354
APPROXIMATE OTHER EQUIVALENTS

IS : 15NiCrMo12 (EN – 353) VISL : M – ECN 170 BASL : B – CH 14 (EN-353)
16NiCr2Mo20 (EN – 354) BASL : B – CH 16 (EN-354)

DIN : 17CrNiM06 AISI – 4317H/4317H BS : 820 M 17

APPLICATION

This Steel possess high tensile Strength of Core Coupled with high toughness. Used for components in Vehicle & Air crafts as well as for General Engineering purposes where Blows & Shocks are Involved Mostly for Gear Box and Transmission Components, Cam Shafts.

Our Colour Code: BLUE & RED

LIST OF STANDARD SIZES

  • Round: Ø 16mm – Ø 350mm

OUR STOCKS

  • EN-353 Round: Ø 18mm – Ø 310mm 
QUALITYCSiMnCrNiMoP & S
EN – 3530.120.10.60.7510.080.04
EN – 3530.180.3511.251.50.15MAX
EN – 3540.120.20.50.751.50.10.04
EN – 3540.180.3511.2520.25MAX
SPECIFIC HEAT TREATMENT
QUALITYEN – 353 & EN 354
Forging Temperature1050 to 850ºC
Annealing Temperature640 to 890ºC (Soft Annealing)
Annealed Hardness BHN Max217 BHN
Hardening Temperature840 to 870ºC & 800 to 830ºC R&H
Quenching MediaOil / Salt Bath
Obtainable Hardness R.C.—-
Working Hardness HRC.—-
Tempering Temperature170 to 210ºC
Normalising Temperature830 to 875ºC